ASTM A334 GR. 6 tiub lancar suhu rendah
dapatkan harga terkiniJenis bayaran: | L/C,T/T,D/P |
Incoterm: | FOB,CFR,CIF,EXW |
Pengangkutan: | Express,Land,Ocean |
Port: | Tianjin,Shanghai,Qingdao |
Jenis bayaran: | L/C,T/T,D/P |
Incoterm: | FOB,CFR,CIF,EXW |
Pengangkutan: | Express,Land,Ocean |
Port: | Tianjin,Shanghai,Qingdao |
Model No.: ASTM A334 Gr. 6
Standard: bs, GB, ASTM, JIS, MAKAN, API
Bahan: A53-A369, Q195-Q345, 10 # -45 #, Aloi Mn-V, Aloi CrNi, Aloi Cr-Mo
Bentuk Bahagian: Bulat
Tempat Asal: China
Permohonan: Paip Bendalir, Paip Dandang, Paip Struktur
Proses Pengeluaran: Hot Rolled
Persijilan: API, pejabat
Tiub Khas: Pipa Dinding Tebal
Sama Ada Aloi: Adakah Aloi
Bertolak Ansur: ± 1%
Kategori: Paip Keluli lancar
Perkhidmatan Pemprosesan: Keratan, Menumbuk, Menyahtapis, Kimpalan, Membengkok
Unit Jualan | : | Ton |
Jenis Pakej | : | Pembungkusan marin standard, atau seperti yang dikehendaki oleh pelanggan |
Contoh Gambar | : |
The file is encrypted. Please fill in the following information to continue accessing it
ASTM A334 Gr.6 tiub keluli lancar
Astm A334 Gr.6 Tiub keluli lancar adalah tiub keluli karbon suhu rendah yang digunakan untuk mengangkut cecair pada suhu rendah.
Astm A334 Gr.6 Tiub keluli lancar sesuai digunakan dalam dandang, kapal tekanan, dan penukar haba. Mereka dihasilkan menggunakan keluli karbon berkualiti tinggi dan direka untuk menahan suhu rendah dan tekanan tinggi. Tiub ini mempunyai ketepatan dimensi yang sangat baik dan boleh didapati dalam pelbagai saiz dan ketebalan untuk memenuhi keperluan khusus aplikasi yang berbeza. ASTM A334 Gr.6 Tiub keluli lancar mempunyai sifat kimpalan yang baik dan boleh dikimpal dengan mudah tanpa sebarang gangguan atau retak.
1.1 Spesifikasi ini meliputi beberapa gred minimum-dinding ketebalan, lancar dan dikimpal, tiub karbon dan keluli aloi yang dimaksudkan untuk digunakan pada suhu yang rendah. Sesetengah saiz produk mungkin tidak tersedia di bawah spesifikasi ini kerana ketebalan dinding yang lebih berat mempunyai kesan buruk terhadap sifat impak suhu rendah.
1.2 Keperluan Tambahan S1 dari sifat pilihan disediakan. Ini hanya terpakai apabila ditentukan oleh pembeli.
Nota 1: Untuk tiub lebih kecil daripada 1/2 inci. [12.7 mm] Dalam diameter luar, nilai pemanjangan yang diberikan untuk spesimen jalur dalam Jadual 1 hendaklah terpakai. Keperluan harta mekanikal tidak digunakan untuk tiub lebih kecil daripada 1/8 inci [3.2 mm] di diameter luar dan dengan ketebalan dinding di bawah 0.015 inci. [0.4 mm].
1.3 Nilai-nilai yang dinyatakan dalam unit paun inci atau unit SI dianggap secara berasingan sebagai standard. Di dalam teks, unit SI ditunjukkan dalam kurungan. Nilai -nilai yang dinyatakan dalam setiap sistem tidak setara tepat; Oleh itu, setiap sistem mesti digunakan secara bebas dari yang lain. Menggabungkan nilai dari kedua -dua sistem boleh mengakibatkan ketidakpatuhan dengan spesifikasi. Unit-unit paun inci hendaklah terpakai melainkan jika penamaan "M" spesifikasi ini ditentukan dalam perintah itu.
1.4 Piawaian ini tidak bermaksud untuk menangani semua kebimbangan keselamatan, jika ada, yang dikaitkan dengan penggunaannya. Adalah menjadi tanggungjawab pengguna standard ini untuk menubuhkan amalan keselamatan, kesihatan, dan alam sekitar yang sesuai dan menentukan kebolehgunaan batasan pengawalseliaan sebelum digunakan.
1.5 Piawaian antarabangsa ini telah dibangunkan selaras dengan prinsip -prinsip yang diiktiraf di peringkat antarabangsa mengenai penyeragaman yang ditubuhkan dalam keputusan mengenai prinsip -prinsip untuk pembangunan piawaian, panduan dan cadangan antarabangsa yang dikeluarkan oleh Jawatankuasa Perdagangan Perdagangan Dunia untuk Perdagangan (TBT).
Paip ASTM A333 Gred 6 bersamaan dengan beberapa piawaian antarabangsa termasuk EN/DIN 10216-2, BS 3059 Bahagian 2, dan ASME SA-106.
ASTM A334 / ASME SA334 Gred 6 Komposisi Kimia
Standard |
Grade |
Chemical Components (%) |
|||||
C |
Si |
Mn |
P |
S |
Ni |
||
ASTM A334/ ASME SA334 |
GR.6 |
≤0.30 |
≥0.10 |
0.29-1.06 |
≤0.025 |
≤0.025 |
/ |
Ujian mekanikal diperlukan
Standard |
Grade |
Mechanical Properties |
|||
Tensile |
Yield |
Elongation |
The Low degree of Temperature test |
||
Strength (Mpa) |
Strength (Mpa) |
(%) |
|||
ASTM A334/ ASME SA334 |
Gr.6 |
≥415 |
≥240 |
≥30 |
-45° |
Nombor kekerasan maksimum
Grade |
Rockwell |
Brinell |
ASTM A334 Grade 6 |
B90 |
190 |
Keperluan Kesan A334 Gr.6
Size of Specimen, mm |
Minimum Average Notched Bar Impact Value of. Each Set of Three Specimens |
Minimum Notched Bar Impact Value of One Specimen Only of a Set |
||
ft·lbf |
J |
ft·lbf |
J |
|
10 by 10 |
13 |
18 |
10 |
14 |
10 by 7.5 |
10 |
14 |
8 |
11 |
10 by 6.67 |
9 |
12 |
7 |
9 |
10 by 5 |
7 |
9 |
5 |
7 |
10 by 3.33 |
5 |
7 |
3 |
4 |
10 by 2.5 |
4 |
5 |
3 |
4 |
A334 Gr.6 Pengurangan suhu kesan:
Specimen Width Along Notch or Accrual Material Thickness |
Temperature Reduction, Degrees Colder |
||
In. |
mm |
℉ |
℃ |
0.394 |
10(Standard size) |
0 |
0 |
0.354 |
9 |
0 |
0 |
0.315 |
8 |
0 |
0 |
0.295 |
7.5(3/4 std. size) |
5 |
3 |
0.276 |
7 |
8 |
4 |
0.262 |
6.67(2/3 std. sze) |
10 |
5 |
0.236 |
6 |
15 |
8 |
0.197 |
5(1/2 std. size) |
20 |
11 |
0.158 |
4 |
30 |
17 |
0.131 |
3.33(1/3 std. size) |
35 |
19 |
0.118 |
3 |
40 |
22 |
0.099 |
2.5(1/4 std. size) |
50 |
28 |
Ujian meratakan Satu ujian meratakan hendaklah dibuat pada spesimen dari setiap hujung satu tiub selesai setiap lot.
Ujian suar (tiub lancar) Satu ujian suar hendaklah dibuat pada spesimen dari setiap hujung satu tiub selesai setiap lot.
Ujian Flange (tiub dikimpal) Satu ujian bebibir hendaklah dibuat pada spesimen dari setiap hujung satu tiub selesai setiap lot.
Ujian meratakan terbalik untuk tiub yang dikimpal, satu ujian meratakan semula akan dibuat pada spesimen dari setiap 1500 kaki [460 m] tiub selesai.
Ujian kekerasan Brinell atau ujian kekerasan Rockwell hendaklah dibuat pada spesimen dari dua tiub dari setiap lot (Nota 3).
Ujian Impak Satu ujian impak bar bertali, yang terdiri daripada melanggar tiga spesimen, hendaklah dibuat dari setiap haba yang diwakili dalam beban rawatan haba pada spesimen yang diambil dari tiub siap.
ASTM A334 / ASME SA334 GR.6 tiub hidrostatik atau ujian NDT
Setiap tiub A334 gr.6 hendaklah tertakluk kepada ujian elektrik yang tidak menentu atau ujian hidrostatik. Jenis ujian yang akan digunakan hendaklah pada pilihan pengilang, melainkan dinyatakan sebaliknya dalam perintah pembelian.
Semua A334 Gr.6 tiub lancar dan dikimpal, selain daripada gred 8 dan 11, hendaklah dirawat untuk mengawal mikrostruktur mereka dalam accor-tarian dengan salah satu kaedah berikut:
ASTM ASME A/SA334 GR.6 Pesanan tiub lancar untuk bahan di bawah spesifikasi ini hendaklah termasuk yang berikut, seperti yang diperlukan, untuk menggambarkan bahan yang mencukupi:
Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.
Fill in more information so that we can get in touch with you faster
Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.